Optimum Heat Treatment of Extrusion Die Steel

Article Preview

Abstract:

Commercial hot extrusion is a billet-by-billet cyclic process, with high thermal and mechanical stresses generated in the die set. The die is a costly piece of equipment, and its long service life is essential for profitable operation. Extrusion dies primarily fail by fracture, wear, and plastic deformation. To avoid early failure, it is essential to have an optimum combination of toughness and hardness in the die. This combination can be achieved through a judicious mix of heat treatment and surface hardening. Experiments were conducted to determine mechanical properties of H13 steel after various heat treatment sequences. Heat treatment strategy is described in detail, and effect of different tempering temperatures on fracture toughness and hardness of the tool steel is reported. Changes in mechanical properties are also related to the variation in microstructure. For use in commercial hot extrusion dies, optimum tempering temperature for H13 steel was found to be near 525-600oC, for the best combination of toughness and hardness.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

215-219

Citation:

Online since:

March 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Arif A.F.M., Sheikh A.K., Qamar S.Z., al-Fuhaid K.M., Modes of Die Failure and Tool Complexity in Hot Extrusion of Al-6063, Journal of Materials Processing Technology, 134 (3), 2003, pp.318-328.

DOI: 10.1016/s0924-0136(02)01116-0

Google Scholar

[2] ASM International, ASM Metals Handbook Volume 1: Properties and Selection: Irons, Steels, and High-Performance Alloys, 10th edition, ASM International, (1990).

DOI: 10.31399/asm.hb.v01.9781627081610

Google Scholar

[3] Totten GE (ed) Steel Heat Treatment Handbook: Volumes I and II, 2nd edition, CRC Press, Taylor and Francis Group, (2007).

Google Scholar

[4] Bryson WE, Heat Treatment, Selection, and Application of Tool Steels, 2nd edition, Hanser Gardner Publications, (2005).

Google Scholar

[5] ASM International, ASM Handbook Volume 4: Heat Treating, ASM International, (2006).

Google Scholar

[6] Hu X., Li L., Wu X., Zhang M., Coarsening Behavior of M23C6 Carbides after Ageing or Thermal Fatigue in AISI H13 Steel with Niobium, International Journal of Fatigue, 28 (3), 2006, pp.175-182.

DOI: 10.1016/j.ijfatigue.2005.06.042

Google Scholar

[7] Rodenburg C., Rainforth W.M., A Quantitative Analysis of the Influence of Carbides Size Distributions on Wear Behaviour of High-Speed Steel in Dry Rolling/Sliding Contact, Acta Materialia, 55 (7), 2007, p.2443–2454.

DOI: 10.1016/j.actamat.2006.11.039

Google Scholar

[8] Qamar S.Z., Sheikh A.K., Arif A.F.M., Pervez T., Regression-Based CVN-KIC Models for Hot Work Tool Steels, Materials Science and Engineering A, 430 (1-2), 2006, pp.208-215.

DOI: 10.1016/j.msea.2006.05.103

Google Scholar