The Oxide Defect of C70250 Alloy
Abstract:
The oxide skin defect during hot rolling process for Cu-Ni-Si alloy strip was investigated. Oxide skin defects were analyzed by means of alloy elements detection and microstructures characterization. The characterization and test results showed that high temperature oxidation and silicon segregation are the main causes of the oxide skin defect. Pilot scale tests indicated that hot processing temperature for C70250 alloy should be lower than 950°C. Reducing atmosphere is recommended during the thermal treatment of Cu-Ni-Si alloys.