Application of Calculus Equation in Solving Thermal Decomposition Kinetics Parameters of Flame Retardant Wood

Article Preview

Abstract:

Wood has been treated with amino resins and amino resins modified with phosphoric acid to impart flame retardancy. The thermal degradation of samples has been studied by thermogravimetry (TG) in air. From the resulting data, kinetic parameters for different stages of thermal degradation are obtained following the method of Broido. For the decomposition of wood and flame retardant wood, the activation energy is found to decrease from 122 to 72 kJmol-1.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

190-193

Citation:

Online since:

June 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Goldstein, I. S. and Dreher, W. A., 1964, U. S. 3, 159, 503.

Google Scholar

[2] Juneja, S. C., 1975, U. S. 3, 887, 511.

Google Scholar

[3] Bhagwan, J. and Lal, K., 1990, J. Polym. Mater. 7, 231.

Google Scholar

[4] Gao, M. Zhu, K. and Sun, Y. C., J. Fire Sci., 22(6) (2004) 505.

Google Scholar

[5] Gao, M. Li, S. Y. and Sun, Y. C., Combustion Science and Technology, 176(12), (2004) (2057).

Google Scholar

[6] Broido, A., 1969, J. Polym. Sci. Part A-2, 7, 1761.

Google Scholar