Study on the Evolution of Defects in Helium-Implanted Tungsten

Article Preview

Abstract:

The microstructure of He+-irradiation induced defects in tungsten was studied as functions of annealing temperature by means of scanning electron microscope (SEM) and Doppler broadening positron annihilation spectroscopy (DB-PAS). The results show that the S parameter become higher after helium implanted in tungsten. When the annealing temperature increases to 923 K, plenty of large size of holes and new types of defects could be found in this sample.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

100-103

Citation:

Online since:

March 2017

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2016 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] G. Federici, V. Barabash, G. Janeschitz, R. Tivey, Selection of plasma-facing materials in next-step fusion devices[C]/, Fusion Engineering, 19th Symposium on. IEEE, p.311(2002).

DOI: 10.1109/fusion.2002.1027701

Google Scholar

[2] H. Bolt, V. Barabash, G. Federici, J. Linke J, A. Loarte, A. Roth, K. Sato, Plasma facing and high heat flux materials–needs for ITER and beyond, J. Nucl. Mater. 307 (2002) 43-52.

DOI: 10.1016/s0022-3115(02)01175-3

Google Scholar

[3] YUAN Baoshan, JIANG Shaofeng, LU Zhihong, Device Foundation of Tokamak, (Beijing, Atomic Energy Press, 2011) pp.155-168.

Google Scholar

[4] R.S. Barnes, Embrittlement of stainless steels and nickel-based alloys at high temperature induced by neutron radiation, Nature, 206 (1965).

DOI: 10.1038/2061307a0

Google Scholar

[5] K.B. Woller, D.G. Whyte, G.M. Wright, R.P. Doerner, G. De Temmerman, Helium concentration in tungsten nano-tendril surface morphology using Elastic Recoil Detection, J. Nucl. Mater. 438 (2013) S913-S916.

DOI: 10.1016/j.jnucmat.2013.01.198

Google Scholar

[6] H. Iwakiri, K. Yasunaga, K. Morishita, N. Yoshida, Microstructure evolution in tungsten during low-energy helium ion irradiation, J. Nucl. Mater. 283 (2000) 1134-1138.

DOI: 10.1016/s0022-3115(00)00289-0

Google Scholar

[7] A. Debelle, M.F. Barthe, T. Sauvage, First temperature stage evolution of irradiation-induced defects in tungsten studied by positron annihilation spectroscopy, J. Nucl. Mater. 376 (2008) 216-221.

DOI: 10.1016/j.jnucmat.2008.03.002

Google Scholar

[8] P.E. Lhuillier, T. Belhabib, P. Desgardin, B. Courtois, T. Sauvage, M.F. Barthe, A.L. Thomann, P. Brault, Y. Tessier, Trapping and release of helium in tungsten, J. Nucl. Mater. 416 (2011) 13-17.

DOI: 10.1016/j.jnucmat.2010.12.042

Google Scholar

[9] J.F. Ziegler, J.P. Biersack, SRIM-2008, Stopping Power and Range of Ions in Matter(2008).

Google Scholar