The Influence of Indentation Conditions on Nanohardness Depth Profiles of W-C Based Coatings

Article Preview

Abstract:

The influence of different indentation parameters including loading type, loading/strain rate, frequency and amplitude on nanohardness depth profiles on DC-MS W-C based coatings thick from 300 to 850 nm were investigated with the aim to determine the best conditions for the measurement of hardness of thin films during sinusoidal loading cycle. Nanohardness tests were performed on G200 (Agilent Technologies) and NHT (CSM Instruments) nanoindenters using standard loading/unloading cycle, CMC (continuous multicycle) mode and continuous stiffness measurement method (CSM) or sinus mode, respectively. The increase of strain rate and sinus amplitude results in decrease of maxima hardness of profiles while the increase of frequency caused its increase.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

175-178

Citation:

Online since:

March 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] G.M. Pharr, W.C. Oliver, On the generality of the relationship among contact stiffness, contact area and elastic modulus during indentation, J. Mater. Res. 3 (1992) 613 – 617.

DOI: 10.1557/jmr.1992.0613

Google Scholar

[2] Information on: http: /www. perkinelmer. com/CMSResources/Images/44-74546GDE_IntroductionToDMA. pdf.

Google Scholar

[3] Sinus mode guidelines, Information bulletin for manipulation with technical devices, CSM Instruments SA (Switzerland) (2010).

Google Scholar

[4] Sinus mode equations, Sinus mode calculations principles. In CSM Instruments – online bulletin, CSM Instruments SA (Switzerland) (2010) 18 – 20.

Google Scholar

[5] J. Hay, P. Agee, E. Herbert, Continuous stiffness measurement during instrumented indentation testing, Experimental techniques (2010) 86 – 94.

DOI: 10.1111/j.1747-1567.2010.00618.x

Google Scholar

[6] L. Xiaodong, B. Bharat, A review of nanoindentation continuous stiffness measurement technique and its applications, Materials Characterization 48 (2002) 11 – 36.

DOI: 10.1016/s1044-5803(02)00192-4

Google Scholar

[7] P. Hviščová, F. Lofaj, M. Novák, Nanohardness of CrN coatings vs. Deposition parameters, Key Engineering Materials in Local Mechanical Properties 2013, (2014) In press.

DOI: 10.4028/www.scientific.net/kem.606.191

Google Scholar