Investigation of Bonding Strength of Al Solid Phase Diffusion Bonded Joint with Surface Treatment Using Electrolyzed Water

Article Preview

Abstract:

In this study, the effect of surface treatment of Al with alkaline (pH 10.5 and pH 12.4) and acidic (pH 3.7) electrolyzed water was investigated on bonding strength of solid phase diffusion bonded Al. Aluminum hydroxide and hydroxyl groups were appeared on the surface of Al which was treated with alkaline electrolyzed water of pH 12.4 at 323 K for 2700 s. It was found that such treatment is similar to the one with NaOH aqueous solution at 323 K for 30 s. For bonding strength, shear strength of the bonded Al specimens treated with electrolyzed water of pH 12.4 at 293 K for 3 s and 30 s were higher than that of the untreated specimen.

You might also be interested in these eBooks

Info:

Periodical:

Materials Science Forum (Volume 1016)

Pages:

1466-1472

Citation:

Online since:

January 2021

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2021 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Y. Liang, S. Hu, J. Shen, H. Zhang, P. Wang, Geometrical and microstructural characteristics of the TIG-CMT hybrid welding in 6061 aluminum alloy cladding, Journal of Materials Processing Technology, 239 (2017) 18-30.

DOI: 10.1016/j.jmatprotec.2016.08.005

Google Scholar

[2] H. R. Hazari, M. Balubai, D. S. Kumar, A. U. Haq, Experimental investigation of TIG welding on AA 6082 and AA 8011, Materials Today: Proceedings 19 (2019) 818-822.

DOI: 10.1016/j.matpr.2019.08.137

Google Scholar

[3] X. Zhan, Y. Zhao, Z. Liu, Q. Gao, H. Bu, Microstructure and porosity characteristics of 5A06 aluminum alloy joints using laser-MIG hybrid welding, Journal of Manufacturing Processes, 35 (2018) 437-445.

DOI: 10.1016/j.jmapro.2018.08.011

Google Scholar

[4] J. Liu, H. Zhu, Z. Li, W. Cui, Y. Shi, Effect of ultrasonic power on porosity, microstructure, mechanical properties of the aluminum alloy joint by ultrasonic assisted laser-MIG hybrid welding, Optics and Laser Technology, 119 (2019) 105619.

DOI: 10.1016/j.optlastec.2019.105619

Google Scholar

[5] C. Cai, S. He, H. Chen, W. Zhang, The influences of Ar-He shielding gas mixture on welding characteristics of fiber laser-MIG hybrid welding of aluminum alloy, Optics and Laser Technology, 113 (2019) 37-45.

DOI: 10.1016/j.optlastec.2018.12.011

Google Scholar

[6] S. Lin, Y.-L. Deng, J.-G. Tang, S.-H. Deng, H.-Q. Lin, L.-Y. Ye, X.-M. Zhang, Microstructures and fatigue behaviour of metal-inert-gas-welded joints for extruded Al-Mg-Si alloy, Materials Science & Engineering A, 745 (2019) 63-73.

DOI: 10.1016/j.msea.2018.12.080

Google Scholar

[7] A.S. Zuruzi, H. Li, G. Dong, Effects of surface roughness on the diffusion bonding of Al alloy 6061 in air, Materials Science and Engineering A, 270 (1999) 244-248.

DOI: 10.1016/s0921-5093(99)00188-4

Google Scholar

[8] H.-Y. Wu, S. Lee, Y.-H. You, Genuine solid-state bonding characteristics of superplastic Al-alloys, Journal of Materials Processing Technology, 122 (2002) 226-231.

DOI: 10.1016/s0924-0136(02)00006-7

Google Scholar

[9] G. Chen, Q. Shi, Y. Li, Z. Han, K. Yuan, Experimental investigations on the kinetics of void shrinkage in solid state bonding of AA6061 at high temperatures and high pressures, Materials and Design, 89 (2016) 1223-1226.

DOI: 10.1016/j.matdes.2015.10.102

Google Scholar

[10] S. Koyama, T. S. Keat, S. Amari, K. Matsubara, I. Shohji, Effect of surface modification by aqueous NaOH solution on bond strength of solid-state bonded interface of Al, Materials Transactions, 54 (2013) 1975-1980.

DOI: 10.2320/matertrans.m2013101

Google Scholar

[11] T. Ohwaki, Characterization of native oxide on aluminium by infrared spectroscopy, Journal of Japan Institute of Light Metals, 54 (2004) 31-36.

Google Scholar

[12] W. Suetaka, Infrared absorption spectra of the chemical conversion coating films of aluminium, Journal of Japan Institute of Metals, 32 (1968) 1233-1237.

Google Scholar

[13] Y. Shimizu, K. Yamada, Corrosion and corrosion control of aluminium, Journal of Japan Institute of Light Metals, 26 (1976) 356-377.

Google Scholar

[14] G. Itoh, Corrosion of aluminium, Journal of Japan Institute of Light Metals, 31 (1981) 683-696.

Google Scholar