High Temperature Oxidation of TiAl(La)N Coating Deposited on a Steel Substrate by Arc-Ion Plating

Article Preview

Abstract:

The high temperature oxidation behavior of the TiAl(La)N coating, which was deposited on a steel substrate by the arc-ion plating method, was investigated at 700, 800 and 900oC in atmospheric air. The oxidation kinetics of the coating were mainly governed by the inward diffusion of oxygen and outward transport of nitrogen. The oxide scale was porous, nonadherent, and prone to cracking, indicating the oxidation resistance above 700oC is poor.

You might also be interested in these eBooks

Info:

Periodical:

Materials Science Forum (Volumes 510-511)

Pages:

410-413

Citation:

Online since:

March 2006

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2006 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] L. Rebouta, F. Vaz, M. Andritschky, M.F. da Silva: Surf. Coat. Technol. Vol. 76-77 (1995) p.70.

Google Scholar

[2] L.A. Donohue, I.J. Smith, W. -D. Muenz, I. Petrov, J.E. Greene: Surf. Coat. Technol. Vol. 94-95 (1997) p.226.

Google Scholar

[3] F. Vaz, L. Rebouta, M. Andritschky, M.F. da Silva, J.C. Soares: Surf. Coat. Technol. Vol. 98 (1998) p.912.

Google Scholar

[4] K.S. Lee, S.M. Seo, K.A. Lee: Script. Mater. Vol. 52, (2005) p.445.

Google Scholar

[5] H. Ichimura, A. Kawana: J. Mater. Res. Vol. 8 (1993) p.1093.

Google Scholar