Oxidation Kinetics of ZrB2 Ceramic Matrix Composite Materials

Article Preview

Abstract:

Zirconium diboride is widely applied because of some excellent performances. The oxidation kinetics of ZrB2-YAG-Al2O3 composite materials were researched, which helps to improve the performance of ultra-high-temperature composite materials. The results show the oxidation weight gain is decreased with increasing the content of YAG-Al2O3 and the molar ratio of Al2O3. The oxidation weight gain is increased with prolonging the oxidation time under 1300°Cæ, the oxidation weight gain ratio is decreased with prolonging the oxidation time. The effecting tendency of oxidation weight gain is not abvious with varying the contend of YAG-Al2O3 upon 1300°Cæ, however, the effecting tendency of oxidation weight gain is very abvious with varying the molar ratio of Al2O3.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

116-120

Citation:

Online since:

July 2017

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2017 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] S.M. Zhang, S. Wang, Y.L. Zhu, Fabrication of ZrB2-ZrC-based composites by reactive melt infiltration at relative low temperature, Scripta Mater. 65 (2011) 139-142.

DOI: 10.1016/j.scriptamat.2011.03.033

Google Scholar

[2] J. Watts, G. Hilmas, W.G. Fahrenholtz, Measurement of thermal residual stresses in ZrB2-SiC composites, J. Eur. Ceram. Soc. 31 (2011) 1811-1820.

DOI: 10.1016/j.jeurceramsoc.2011.03.024

Google Scholar

[3] Y.H. Huang, D.L. Jiang, J.X. Zhang, Sintering kinetics of YAG composite materialss, J. Rare Earth 32(2014) 416-422.

Google Scholar

[4] R. Marder, C. Estournes, G. Chevallier, Spark and plasma in spark plasma sintering of rigid composite materials nanoparticles: A model system of YAG, J. Eur. Ceram. Soc. 35(2015) 211-218.

DOI: 10.1016/j.jeurceramsoc.2014.08.001

Google Scholar

[5] S. Singh, R. Singh, Effect of process parameters on micro hardness of Al-Al2O3 composite prepared using an alternative reinforced pattern in fused deposition modelling assisted investment casting, Rob. Comp. Integ. Manuf. 37 (2016) 162-169.

DOI: 10.1016/j.rcim.2015.09.009

Google Scholar

[6] M. Ashida, Z. Horita, Effects of ball milling and high-pressure torsion for improving mechanical properties of Al-Al2O3 nanocomposites, J. Mater. Sci. 47 (2012) 7821-7827.

DOI: 10.1007/s10853-012-6679-5

Google Scholar

[7] H.J. Zhou, L. Gao, Z. Wang, S. M Dong, ZrB2-SiC oxidation protective coating on C/C Composites prepared by vapor silicon infiltration process, J. Am. Ceram. Soc. 93 (2010) 915-919.

DOI: 10.1111/j.1551-2916.2009.03481.x

Google Scholar

[8] J.G. Song, F. Wang, M.H. Xu, Shibin Li, Effect of adding phase on the properties of ZrB2 based ultra-high-temperature composite materialss. Key Eng. Mater. 512 (2012) 735-738.

Google Scholar

[9] W.M. Guo, Z.G. Yang, G.J. Zhang, Microstructural evolution of ZrB2-MoSi2 composites during heat treatment, Ceram. Int. 37 (2011) 2931-2935.

DOI: 10.1016/j.ceramint.2011.03.027

Google Scholar

[10] C.Y. Tian, D. Gao, Y. Zhang, C.L. Xu. Oxidation behaviour of zirconium diboride-silicon carbide composite materials composites under low oxygen partial pressure, Corros. Sci. 53 (2011) 3742-3746.

DOI: 10.1016/j.corsci.2011.07.020

Google Scholar