The Ultra Fine Grained (UFG) Zn Produced by Ball Milling

Abstract:

Article Preview

Bulk ultra fine grained (UFG) Zn was produced by in situ consolidation of Zn elemental powder with ball milling at room temperature and annealed for 1 hour at 200 after pure Zn milled. The 150 % elongation is obtained in UFG Zn during tensile test at 20 which is equal to 0.43 Tm (Tm is the melting temperature of pure Zn). The elongation of UFG Zn is higher than the 110 % elongation of nanocrystalline Zn ball milled at tensile elongation. The largest tensile elongation (150%) was observed at room temperature in UFG Zn.

Info:

Periodical:

Solid State Phenomena (Volume 118)

Edited by:

Jang Hyun Sung, Chan Gyu Lee, Yong Zoo You, Young Kook Lee and Jae Young Kim

Pages:

609-614

DOI:

10.4028/www.scientific.net/SSP.118.609

Citation:

X. K. Zhu et al., "The Ultra Fine Grained (UFG) Zn Produced by Ball Milling ", Solid State Phenomena, Vol. 118, pp. 609-614, 2006

Online since:

December 2006

Export:

Price:

$35.00

In order to see related information, you need to Login.

In order to see related information, you need to Login.