Authors: Lily Pudjiastuti, Achmad Dwitama Karisma, Jauharatul Wardah, Soeprijanto Soeprijanto, Daril Ridho Zuchrillah, Niniek Fajar Puspita, Shofi’atin Nazilah
The amorphous carbon structure was obtained at the diffraction angle of 23o.
It shows that the carbon structure is fiber-like with a tubular shape.
It shows that the structure of the activated carbon is an irregular shape.
Moreover, activated carbon has a rich pore structure.
College of Chemistry and Chemical Engineering, Southwest Petroleum University, Chengdu, 610500, PR China. (2021). https://doi.org/10.1016/j.jhazmat.2020.123579 [5] T.
Online since: November 2011
Authors: Yin Er Wang, Chao Qiong Zhao, Xiao Wu Wang
Pure molecule of NPG, PE or TRIS has layer-shaped structure.
Structure difference between NPG and PE is the biggest, so the hydrogen bond is affected more serious.
Structure difference between TRIS and PE is the smallest, so there shows a different case.
This is because PE and TRIS are close in crystal structure, atom mass and atom size.
Because hydrogen bonds are influenced by the structure defects, there is no uniform trend between the value of x and specific capacity.
Online since: March 2021
Authors: Wan Mohd Nazri Wan Abdul Rahman, Nor Yuziah Mohd Yunus, Siti Noorbaini Sarmin, Nur Sakinah Mohamed Tamat
Lignin forms a protective covering around the cellulose structure and closely intermingled.
It has amorphous structure and hydrophilic characteristic.
The structure bound together by hemicellulose and lignin [27].
Krausz, Influence of various chemical treatments on the composition and structure of hemp fibres. 
Journal of wood chemistry and technology, 28(3) (2008) 207-226
Online since: August 2018
Authors: Wen Zhong Lu, Fei Liang, Zi Qing Zeng, Gui Fen Fan, Xiao Hong Wang, Meng Meng Hao
This can be explained by the different structures of the calcination precursors.
We can obtain different precursor structures with different n()/n(Y3+).
Three-layer core-shell structure had shortened the diffusion distance of Y3+ and Al3+.
Dean, section 5, Physical properties, in: Lange's handbook of chemistry, World Publishing Company, Beijing, 2003, pp. 639-662
Panjepour, Effect of mechanical activation on structure and thermal decomposition of aluminum sulfate, J.
Online since: February 2011
Authors: Hai Xia Liu, Sheng Jie Li, Yong Nian Yan
The technology can form a predefined three-dimensional structure with certain shape and size, suitable for variety of natural polymer materials (the most similar with extracellular matrix, such as fibrin, sodium alginate, chitosan, hyaluronic acid) with gelatin coupling forming; therefore, it satisfied majority cells needs of choosing the gelatin-based composite hydrogels reasonably.
Tissue analog precursor should mimic the natural organizations farthest in the structure and function [3], therefore, it should have suitable shape and gradient distribution in macro structure, should have vascular-like systems for transmission the nutrients and metabolic residue in micro structure, materials also need to have diversity available for cell selection.
Based on the technology, more complex 3D structures can be manufactured, both the macro structure forming and micro pore constructing can be coupled to the same forming process, the structure shape and pore is more controllable, the process is relatively easy to information [11-12].
The biomaterials applied to cell assembly should have the bionic features in composition and structure, were chosen according to two aspects: (i) should be compatible with cells, suitable for cell survival, growth, and proliferation (i.e., water diffusible, biodegradable, and biocompatible) and (ii) should be easily processed and shaped without causing harm to the cells.
Scherer: Sol-gel science: the physics and chemistry of sol-gel processing.
Online since: November 2012
Authors: Juha Larismaa, Simo Pekka Hannula, Outi Söderberg, Jesse Syrén, Eero Haimi
.% of silver in the structure and the diameter of the silver particles on the silica carriers was 30 ± 7 nm on average.
Depending on the annealing temperature after the air-drying, the structure of both silver and silica vary.
The crystal structure of the powder was examined by q-2q XRD measurements (Philips PW1710) using CuKa radiation.
Processing provides a porous silica structure that holds together, and has quite similar silver structure as the powder applied.
Iler, Chemistry of Silica: Solubility, Polymerization, Colloid and Surface Properties and Biochemistry, John Wiley & Sons, New York, 1979
Online since: August 2014
Authors: Wei Dong Liu, Yun Hong Ding, Jin Chang, Ke Xu
Long chain sulfur compound break down into small molecules, damaging the colloidal structure of heavy oil, improving the quality of heavy irreversible.
By the means of pyrolysis, the colloidal structure in resins was damage to disintegrate between saturates and aromatics. 2.2 Sub-critical water modification Sub-critical water is a new medium and a good solvent being developed under the idea of green chemistry.
(2) The fA in SWM, CM and CMH decreased, indicating the degree of Aromatic structure lower in modification process, such as heavy oil colloidal system was destroyed, and aggregates dispersed into small degree and aromatic structure.
Long chain sulfur compound break down into small molecules, damaging the colloidal structure of heavy oil, improving the quality of heavy irreversible
Average structure parameter in Tarim heavy oils and their sub-fractions.
Online since: September 2021
Authors: Jia Zhen Wang, Jing Du, Yun Bo Wang
It tends to form a very thin and loose structure attached to the beaker wall.
What's more, the high porosity can also mean the confusion of the structure of the backbone of our system, and the confusion of the structure will increase the heat resistance of our system.
SEM pictures show similar structures too.
They also show similar spherulitic crystal structures (see Fig. 3 (a), (b), (c), (d)).
Carraher, and Raymond Benedict Seymour 2003 Seymour/Carraher's polymer chemistry.
Online since: April 2021
Authors: Andrea Ghiotti, Stefania Bruschi, Marco Sorgato, Lucia Lizzul
The pretreatments techniques herein assessed were the metal sheet annealing to change the surface chemistry, and the metal sheet mechanical abrasion by sandblasting with the aim to increase the surface roughness.
The microstructural and mechanical results were then correlated to the metal sheet surface morphology and chemistry induced by the different treatments examined through optical profilometry and X-ray Photoelectron Spectroscopy (XPS).
A steel structure supported a screw, which, employing a pre-compressed spring with a load cell, allowed applying a normal force (FN) on the samples through a steel punch.
The Authors also assume that the Sdr parameter cannot describe the porous structure of the oxide layer since this parameter cannot be used to accurately evaluate reentrant surfaces [16].
Laser-generated macroscopic and microscopic surface structures for the joining of aluminum and thermoplastics using friction press joining.
Online since: October 2016
Authors: Pelagia Glampedaki
As previously mentioned, total absorption times are drastically improved by both PNIAA microgel and CM complexes that facilitate water absorption in their own structure.
Shahinpoor, H-J Schneider H-J (Eds.), Intelligent Materials, Royal Society of Chemistry, Cambridge (2008) [2] MW.
Structural evolution and structure analysis (1st Ed.), Plenum Press, New York (1998) [5] MJ.
Luo, Journal of Materials Chemistry 21, (2011) p. 6113 [6] CMA Ashruf, Sensor Review 22, (2002) p. 322 [7] W.
Li, Smart Materials and Structures 19, 035007 (2010) [24] BS.