Authors: Ge Wang, Yu Ying Zhu, Xing Hua Wang, Qiang Li, Yun Hua He
Table 1 DSC data of Ti50Fe22Ni22Sn6 at constant heating rate from 5 to 40K/min
Φ [K.min-1]
Tg [K]
Tx1 [K]
ΔTx1 [K]
Tp1 [K]
Tp2 [K]
Tp3 [K]
10
691
784
93
838
882
916
20
693
798
105
847
896
936
30
696
802
106
851
897
939
40
699
810
110
860
900
942
From Table 1, it can be seen that all the characteristic temperatures, such as the glass transition temperature, the first crystallization temperature, etc. depend on the heating rate, Φ.
Online since: October 2010
Authors: Waldemar Alfredo Monteiro, E. Vitor, S.J. Buso, C.R. Da Silveira, Juan Alfredo Guevara Carrió
Buso 2
1Presbyterian Mackenzie University, Rua da Consolação, 896, prédio 12, sala 406, Consolação, CEP 01302-907, São Paulo - SP, Brazil
2Institute of Energetic and Nuclear Researches (IPEN), São Paulo - SP, Brazil
atecnologia@mackenzie.br, bjgcarrio@mackenzie.br
Keywords: copper-nickel-aluminum alloys, powder metallurgy, microstructure, structural characterization, electrical properties, mechanical properties.