Abstract:

C/C composites have excellent properties, but it will be rapidly oxidized when temperature is above 500 °C, which limits its applications in high temperature environment. In order to improve Anti-oxidation, using CVD method, a SiC coating is prepared on the surface of C/C composites. We have studied the microstructure of the SiC coating, oxidation resistance and high temperature mechanical properties. The results show that SiC coating has excellent oxidation resistance. When coated sample is oxidized at 1500 °C after 50 hours, its oxidation weight loss rate is only 1.45%, and coated samples can still maintain high mechanical properties at 1200 °C.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

253-256

Citation:

Online since:

November 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Imuta M, Gotoh J. Key Eng Mater, 1999, 164-165:. 439-444.

Google Scholar

[2] Zhang LT, Cheng LF and Xu YD. Aeronaut Manuf Technol (in Chinese), 2003, 1: 24-32.

Google Scholar

[3] Naslain R. Design, Compos Sci Technol, 2004, 64 (2):. 155-170.

Google Scholar

[4] Strife Jr, Sheehan J E. Ceram Bull, 1988, 67 (2):. 369-374.

Google Scholar

[5] Cheng LF, Zhang LT, Xu YD, et al. J Northwestern Polytech Univ (in Chin), 1998, 16 (1): 129-132.

Google Scholar

[6] Deng Shijun High-Performance Ceramic Coating (in Chinese) Beijing: Chemical Industry Press, 2003: 164-172.

Google Scholar

[7] Cheng Lf, Xu Yd and Zhang L T. Carbon, 2000, 38 (10):. 1 493-1 498.

Google Scholar

[8] Thrower P A, Methew G K and Meginnis N J. Carbon, 1982, 20 (6): 465.

Google Scholar

[9] Zhao Jiaxiang, Bradt R C and  walker JR P L.  Carbon. 1985, 23 (l): 15.

Google Scholar