Joining of Ceramic Components in the Green State via LPIM
Abstract:
It has been successfully demonstrated that ceramic materials can be joined in the green state without a second phase by using low pressure injection molded parts. The investigation of the joining interface revealed that a high quality interface can be achieved by carefully adjusting the different manufacturing steps. The use of monomodal particle size distribution in the used powder CT3000SG is inferior to a broader particle size distribution obtained by replacing 33% of the finer alumina powder by coarser CT1200SG. In this way the dewaxing process is significantly improved when the wall thickness of the part exceeds 3 mm. The investigation of the mechanical properties of the joined and sintered parts revealed, that the bending strength of the joined specimens achieved about 80 % of the unjoined, monolithic specimens.
Info:
Periodical:
Pages:
207-210
Citation:
Online since:
November 2007
Authors:
Keywords:
Price:
Сopyright:
© 2007 Trans Tech Publications Ltd. All Rights Reserved
Share:
Citation: