Fabrication and Photocatalytic Performance of Bi2O3 Doped with Fe3+
Abstract:
In this paper, Bi2O3 and Fe3+-doped Bi2O3 photocatalysts with different molar ratio of Bi /Fe (nBi:nFe =100:1,2,3,4) was prepared by paralled flaw co-precipitation method. The prepared photocatalysts were characterized by Brunauer-Emmet Teller (BET) method, X-ray diffraction( XRD) and UV-Vis diffuse reflectance spectroscopy. The results show that 3% Fe3+-Bi2O3 prepared has the highest BET surface area, pore volume, the smallest pore size and the particle average size. 3% Fe3+-Bi2O3 exhibits the best photocatalytic activity. The results of further experiments show that the specific surface area, UV-Vis diffuse reflectance all play an important role in promotion of photocatalytic activity of Bi2O3 nanostructure.
Info:
Periodical:
Pages:
1425-1428
Citation:
Online since:
November 2011
Authors:
Keywords:
Price:
Сopyright:
© 2012 Trans Tech Publications Ltd. All Rights Reserved
Share:
Citation: