Abstract:

The polycrystalline of Sr1xLaxMnO3 (x = 0.11.0) samples were synthesized by solid state reaction method and general sintering. The Sr1xLaxMnO3 powders were calcined and sintered by furnace at 900 K and 1173 K for 3 hours in air atmosphere, respectively. Thermopower of the samples were measured by steady state method at temperature range of 290-520 K in air. The thermopower all samples were increased with increasing the La content substitution.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

343-345

Citation:

Online since:

September 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] M. Wang, K. D. Woo, Impact of Sr2MnO4 preparation process on its electrical resistivity, Energy Conversion and Management 49 (2008) 2409–2412.

DOI: 10.1016/j.enconman.2008.01.020

Google Scholar

[2] K. De, R. Ray, R. N. Panda, S. Giri, H. Nakamura, T. Kohara, The effect of Fe substitution on magnetic and transport properties of LaMnO3, J. of Magnetism and Magnetic Materials 288 (2005) 339–346.

DOI: 10.1016/j.jmmm.2004.09.118

Google Scholar

[3] L. Guangchuan, L. Shuguang, L. Changlong, O. Xiuqin , Preparation of Nanometer La1-xSrxMnO3 and Application in Air-Cathode, J. of Rareearths 25 (2007) 264-267.

DOI: 10.1016/s1002-0721(07)60485-2

Google Scholar

[4] J. A. Souza, J. J. Neumeier, R. K. Bollinger, B. McGuire, C. A. M. dos Santos, H. Terashita. Phy. Review B 76, (2007) 024407-024413

Google Scholar

[5] T. Ohtani, K. Kuroda, K. Matsugami, D. Katoh. J. European Ceramic Society 20 (2000) 2721–2726.

DOI: 10.1016/s0955-2219(00)00224-7

Google Scholar