Study of Damage Mechanisms in Cold-Sprayed 316L-Matrix Composite Coatings Using Novel Impact-Sliding Testing

Article Preview

Abstract:

Cold spray is now well recognized as one of the most powerful and efficient coating process because it is cost-attractive and “green”. However, this process still shows limitations to achieve coatings for highly-demanding service conditions such as those required in certain automotive and/or aircraft applications. Beyond these limitations, cold spray is expected to compete with conventional P/M routes.The present work therefore focussed on the study of damage mechanisms in cold-sprayed AISI 316L and 316L-matrix–Cu composites coatings due to high-loading conditions. Different damage mechanisms could occur depending on the content of Cu particle addition, due to changes in the response of the microstructure to the loading. These mechanisms were studied using the newly-developed “impact-sliding” test. In this test, a steel ball impacts the coating surface at a given frequency, with a fixed angle. The influence of major testing parameters was investigated.Microstructures before and after testing were studied using optical microscopy, scanning electron microscopy (SEM), and microprobe analysis in addition to 3D optical profilometry of impacted areas. Damage mechanisms were seen to be of two types, i.e. plastic deformation and wear. These resulted in decohesion of splats, formation of wear debris and formation of a layer with a tribologically-transformed structure (TTS) at the contact surface.Results showed that cold spray could be claimed to be suitable for the achievement of high-performance coatings for industrial applications provided that the coating microstructure can be controlled. This could be done using a composite approach to the coating composition.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

452-462

Citation:

Online since:

May 2014

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] D. MacDonald, B. Jodoin, Study on the Restoration of Aluminum Aerospace IVD Coatings Using Cold Gas Dynamic Spray, Thermal Spray 2013—Innovative Coating Solutions for the Global Economy, (Proc. of the International Thermal Spray Conference), May 13–15, 2013, Busan, Republic of Korea, 161-165.

DOI: 10.31399/asm.cp.itsc2004p0347

Google Scholar

[2] N. Kurgan, R. Varol, Mechanical properties of P/M 316L stainless steel materials, Powder Technology 201(2010)242–247.

DOI: 10.1016/j.powtec.2010.03.041

Google Scholar

[3] Kurgan, Effects of sintering atmosphere on microstructure and mechanical property of sintered powder metallurgy 316L stainless steel, Materials and Design 52(2013)995–998.

DOI: 10.1016/j.matdes.2013.06.035

Google Scholar

[4] N. Kurgan, Y. Sun, B. Cicek & H. Ahlatci, Production of 316L stainless steel implant materials by powder metallurgy and investigation of their wear properties, Chinese Science Bulletin, May (2012) Vol. 57 No. 15.

DOI: 10.1007/s11434-012-5022-5

Google Scholar

[5] S. Balaji, P. Vijay and A. Upadhyaya, Effect of sintering temperature on the electrochemical, hardness and tribological properties of aluminide-reinforced austenitic stainless steel, Scripta Materialia 56(2007)1063–1066.

DOI: 10.1016/j.scriptamat.2007.02.033

Google Scholar

[6] D. Uzunsoy, Investigation of dry sliding wear properties of boron doped powder metallurgy 316L stainless steel, Materials and Design 31(2010)3896–3900.

DOI: 10.1016/j.matdes.2010.02.053

Google Scholar

[7] S. Raadnui, S. Mahathanabodee, R. Tongsri, Tribological behaviour of sintered 316L stainless steel impregnated with MoS2 plain bearing, Wear 265(2008)546–553.

DOI: 10.1016/j.wear.2007.11.014

Google Scholar

[8] O. Coovattanachai and al. Performance improvement of P/M 316L by addition of liquid phase forming powder, Materials Science and Engineering A 445–446(2007)440–445.

DOI: 10.1016/j.msea.2006.09.105

Google Scholar

[9] A. Sova, D. Pervushin, I. Smurov, Development of multimaterial coatings by cold spray and gas detonation spraying, Surface & Coatings Technology 205(2010)1108–1114.

DOI: 10.1016/j.surfcoat.2010.07.092

Google Scholar

[10] J.M. Shockley, H.W. Strauss, R.R. Chromik, N. Brodusch, R. Gauvin, E. Irissou, J. -G. Legoux, In situ tribometry of cold-sprayed Al-Al2O3 composite coatings, Surface & Coatings Technology 215(2013)350–356.

DOI: 10.1016/j.surfcoat.2012.04.099

Google Scholar

[11] G. Rolland, P. Sallamand, V. Guipont, M. Jeandin, E. Boller, C. Bourda, Laser-induced damage in cold-sprayed composite coatings, Surface & Coatings Technology 205(2011)4915–4927.

DOI: 10.1016/j.surfcoat.2011.04.103

Google Scholar

[12] P. Coddet, C. Verdy, C. Coddet, F. Lecouturier, F. Debray, Mechanical properties of Cold Spray deposited NARloy-Z copper alloy, Surface & Coatings Technology (2013) in Press.

DOI: 10.1016/j.surfcoat.2013.06.062

Google Scholar

[13] M. Bashirzadeh, F. Azarmi, C.P. Leither, G. Karami, Investigation on relationship between mechanical properties and microstructural characteristics of metal matrix composites fabricated by cold spraying technique, Applied Surface Science 275(2013).

DOI: 10.1016/j.apsusc.2012.12.166

Google Scholar

[14] M. Messaadi, Ph. Kapsa, Impact-sliding wear of sintered steel at high temperature, Tribologie: approches scientifiques et applications industrielles, Proc. of the 24th JIFT conf., Aix-en-Provence, France, May 9-11, 2012, P. Montmitonnet et al. eds, Presse des Mines, Paris, France, (2013).

Google Scholar

[15] M. Messaadi, G. Bouvard, J. Yang, Ph. Kapsa, Wear of sintered HSS under combined squeeze–sliding lubrication, Wear 301(2013)768–775.

DOI: 10.1016/j.wear.2012.12.022

Google Scholar

[16] C. Langlade & al. , Formation of a TTS layer on Steel Samples by Friction Stir Processing, Proc. of the 26th International Conf. on SMT, Ecole Centrale de Lyon, Ecully, France, June 20-22, 2012, T. S. Sudarshan et al. eds, Valardocs, (2013)483.

Google Scholar

[17] A.C. Sekkal, C. Langlade, A.B. Vannes, Tribologically transformed structure of titanium alloy (TiAl6V4) in surface fatigue induced by repeated impacts, Materials Science and Engineering A 393(2005)140–146.

DOI: 10.1016/j.msea.2004.10.008

Google Scholar

[18] E. Sauger, S. Fouvry, L. Ponsonnet, Ph. Kapsa, J.M. Martin, L. Vincent, Tribologically transformed structure in fretting, Wear 245(2000)39–52.

DOI: 10.1016/s0043-1648(00)00464-6

Google Scholar