Preparation of Sialon/Si3N4-SiC Composite Refractories Using Kyanite Tailings
Abstract:
Sialon-SiC composite powders were synthesized from kyanite tailings through the carbothermal reduction nitridation (CRN) technique. Using Sialon-SiC composites to substitute Si3N4 composites via the CRN technique synthesize Sialon/Si3N4-SiC composite refractories. The phase composition, cross section morphology, and the substituent amount of Sialon-SiC composites impact on refractories mechanical properties were investigated, respectively. The optimized synthesis temperature for the CRN reaction was found to be 1550 °C for 4 h with the excess carbon 20%. The substituent amount of Sialon-SiC was 25%, the mechanical properties of Sialon/Si3N4-SiC composite refractories reached optimal performance, which bending strength value was 41.8 MPa and compression strength value was 61.6 MPa.
Info:
Periodical:
Pages:
467-471
Citation:
Online since:
July 2016
Authors:
Price:
Сopyright:
© 2016 Trans Tech Publications Ltd. All Rights Reserved
Share:
Citation: