Fabrication of Fe-Based Glassy Cores with High Saturation Magnetization and Good Soft Magnetic Properties by Spark Plasma Sintering

Article Preview

Abstract:

Glassy Fe77Ga3P9.5C4B4Si2.5 alloy powders were synthesized in the particle size range below 125 µm by Ar gas atomization. A glassy alloy disc of 10 mm in diameter and 3 mm in thickness with a high relative density of 99.7 % was synthesized by spark plasma sintering. The resulting glassy magnetic core exhibits good soft magnetic properties, i.e., 1.35 T for saturation magnetization, 5 A/m for coercive force and 9600 for maximum permeability.

You might also be interested in these eBooks

Info:

Periodical:

Materials Science Forum (Volumes 475-479)

Pages:

3397-3400

Citation:

Online since:

January 2005

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2005 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] T. Egami, P.J. Flanders and C.D. Graham Jr.: Appl. Phys. Lett. Vol. 26(1975), 128.

Google Scholar

[2] H. Fujimori, T. Masumoto, Y. Obi and M. Kikuchi: Jpn. J. Appl. Phys. Vol. 13(1974), 1889.

Google Scholar

[3] R.C. Sherwood, E.M. Gyorgy, H.S. Chen, S.D. Ferris, G. Noman and H.J. Leamy: AIP Conf. Proc. Vol. 24(1975), 745.

Google Scholar

[4] H.S. Chen: Rep. Prog. Phys. Vol. 43(1980) 353.

Google Scholar

[5] R.W. Cahn: Rapidly Solidified Alloys, ed. H.H. Liebermann, (Marcel Dekker, New York, 1993), p.617.

Google Scholar

[6] A. Inoue: Acta Mater., Vol. 48(2000), 279.

Google Scholar

[7] Y. Kawamura, H. Kato, A. Inoue, T. Masumoto: Int. J. Powder Metall. Vol. 33(1997), 50.

Google Scholar

[8] V. Mamedov: Powder Metallurgy Vol. 45(2002), 322.

Google Scholar

[9] B.L. Shen and A. Inoue: J. Mater. Res. Vol. 18(2003), 2115.

Google Scholar

[10] B.L. Shen and A. Inoue: Mater. Trans. Vol. 43(2002), 1235. Fig. 5 Outer morphology of the Fe77Ga3P9. 5C4B4Si2. 5 disc core with the dimension of 10 mm in outer diameter, 4 mm in inner diameter and 2. 5 mm in thickness.

Google Scholar