Diffusion Controlled Abnormal Grain Growth in Ceramics

Abstract:

Article Preview

The grain growth kinetics of silica and calcia doped alumina at 1400oC and their grain boundary complexion is characterized. These data are compared to predictions of both diffusion controlled and nucleation limited interface controlled grain growth theory. It is deduced from the indicators that the mechanism for normal and abnormal grain growth in these aluminas is diffusion controlled.

Info:

Periodical:

Materials Science Forum (Volumes 558-559)

Edited by:

S.-J.L. Kang, M.Y. Huh, N.M. Hwang, H. Homma, K. Ushioda and Y. Ikuhara

Pages:

1227-1236

Citation:

S. J. Dillon and M. P. Harmer, "Diffusion Controlled Abnormal Grain Growth in Ceramics", Materials Science Forum, Vols. 558-559, pp. 1227-1236, 2007

Online since:

October 2007

Export:

Price:

$38.00

[1] S. J . Bennison and B. R. Lawn: Acta Metall., Vol. 37 (1989), p.2659.

[2] J.J. Cao, W.J. MoberlyChan, L.C. De Jonghe, C.J. Gilbert, R.O. Ritchie: J. Am. Ceram. Soc. Vol. 79 (1996), p.461.

[3] C. Scott, M. Kaliszewski, C. Greskovich, and L. Levinson: J. Am. Ceram. Soc., Vol. 85 (2002), p.1275.

[4] S.J. Dillon and M.P. Harmer: in press. J. Am. Ceram. Soc. (2006).

[5] J. E Burke: . J. Am. Ceram. Soc. Vol. 40 (1957).

[6] M. Yan, R. Cannon, and H. Bowen: Ceramic Microstructures '76, edited by R. M. Fulrath, and J. A. Pask Westview Press, Boulder, Co, (1976), p.276.

[7] J.E. Burke and D. Turnbull: Prog. Metal Phys. Vol. 3 (1952), p.220.

[8] Y. J Park, N. -M. Hwang, D. -Y. Yoon: Metall. Mat. Trans. A Vol. 27A (1996), p.2809.

[9] G.S. Rohrer, C.L. Rohrer, and W.W. Mullins: J. Amer. Ceram. Soc. Vol. 84 (2001), p. (2099).

[10] W. Jo, D. -Y. Kim, N. -M. Hwang: J. Am. Ceram. Soc. Vol. 89 (2006), p.2369.

[11] C. -M. Wang, , H. M. Chan M.P. Harmer: J. Am. Ceram. Soc. Vol. 87 (2004), p.378.

[12] M. A. Gülgün, R. Voytovych, I. MacLaren, M. Rühle, R.M. Cannon: Interface Science Vol. 10 (2002), p.1573.

[13] D.R. Clarke, J. Am. Ceram. Soc. Vol. 70 (1987), p.15.

[14] I. -J. Bae, and S. Baik: J. Am. Ceram. Soc. Vol. 80 (1997), p.1149.

[15] Y. -M. Kim, S. -H. Hong, D. -Y. Kim: J. Am. Ceram. Soc., Vol. 83 (2000), p.2809.

[16] S. -Y. Chung, and S. -J. L. Kang: Acta Mater. Vol. 51 (2003), p.2345.

[17] I. MacLaren, R.M. Cannon, M.A. Gülgün, R. Voytovych, N. Popescu-Pogrion, C. Scheu, U. Täffner, M. Rühle: J. Am. Ceram. Soc. Vol. 86 (2003), p.650.

DOI: https://doi.org/10.1111/j.1151-2916.2003.tb03354.x

[18] J.H. Ahn, J. -H. Lee, S. -H. Hong, N. -M. Hwang, D. -Y. Kim, J: Am. Ceram. Soc. Vol. 86 (2003), p.1421.

[19] M.K. Kang, Y. -S. Yoo, D. -Y. Kim, N. -M. Hwang: J: Am. Ceram. Soc. Vol. 83 (2000), p.385.

[20] T. Sano, and G.S. Rohrer: in press in J. Amer. Ceram. Soc.

[21] S. -Y. Choi, and S. -J. L. Kang: Acta Mater. Vol. 52 (2004), p.2937.

[22] S. -Y. Chung, and S. -J.L. Kang J. Am. Ceram. Soc. Vol. 83 (2000), p.2828.

[23] Y. -S. Yoo, H. Kim, D. -Y. Kim: J. Euro. Ceram. Soc. Vol 17 (1997), p.805.

[24] J.S. Wallace, J. -M. Huh, J.E. Blendell, C.A. Handwerker: J. Am. Ceram Soc. Vol. 85 (2002), p.1581.

[25] D.J. Rockosi, E.P. Gorzkowski, P.T. King, A.M. Scotch, H.M. Chan, M.P. Harmer: J. Am. Ceram Soc. Vol. 87 (2004), p.1339.

[26] S.J. Dillon and M.P. Harmer: in press. J. Am. Ceram. Soc. (2006).

[27] S.J. Dillon and M.P. Harmer: in press. J. Am. Ceram. Soc. (2006).

[28] M. -K. Kang, D. -Y. Kim, N.M. Hwang: J. Euro. Ceram. Soc. Vol. 22 (2002), p.603.

[29] J. Harding, K. Atkinson, R. Grimes: J. Am. Ceram. Soc. Vol. 86 (2003), p.554.

[30] T. -T. Fang, J. -T Shuie, and F. -S. Shiau: Mater. Chem. And Phys. Vol. 80 (2003), p.108.

[31] Z. He, and J. Ma: Ceram. Int. Vol. 27 (2001), p.261.

[32] Tang, M., W.C. Carter, R.M. Cannon: Phys. Rev. B Vol. 73 (2006), p.024102.

[33] S.J. Dillon and M.P. Harmer: submitted to Science (2006).

[34] F.J. Alvez: Ph.D. dissertaion, Lehigh University, Bethlehem, Pa (1997).

[35] C.W. Park, and D.Y. Yoon: J. Am. Ceram. Soc. Vol. 85 (2002), p.1585.

[36] M.J. Kim and D.Y. Yoon: J. Am. Ceram. Soc. Vol. 86 (2003), p.630.

[37] J.H. Back, M.J. Kim, D.Y. Yoon: J: Am. Ceram. Soc. Vol. 88 (2005), p.3177.