The Effect of H3BO3 Microaddition on Microstructure of Ni/MgO Sintered Compact by Co-Precipitation Method

Article Preview

Abstract:

In the present work, Ni/MgO powder was prepared by co-precipitation in which CO restore NiO to elemental subtance Ni due to C2O42- was decompose to CO and CO2 at 700°C. As the process of the second sintering, H3BO3 was added into the sintered powder of 700°C and was grinded. Then the powder of H3BO3 added was sintered at 800°C,so that the powder was refined, obviously. Thermogravimetric analysis (TGA) and differential thermal analysis(DTA) was carried out in CO2 flow at 10°C/min. X-ray diffraction (XRD) was carried out on a X-ray diffractometer operated at 20KV and 40mA. The microstructures and morphologies were studied by EPMA and XPS.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

168-171

Citation:

Online since:

March 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2013 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Carnes Corrie L, Stipp Jennifer, Klabunde Kenneth J, and Bonevich John, Synthesis, characterization, and absorption studies of nanocrystalline copper xide nickel oxide [J]. Langmuir 2002, (18):1352-1359

DOI: 10.1021/la010701p

Google Scholar

[2] Tadahiro Kurosaka, Hiromi Matsuhashi, and Kazushi Arata, JOURNAL OF CATALYSIS, 179(1988), 28-35

Google Scholar