Article Preview

Abstract:

Microhardness of various minerals in sinter was tested in order to better production of sinter with high microhardness minerals in WISCO. The results showed that the hematite microhardness was highest and the glass phase microhardness was lowest, the various minerals microhardness from highest to lowest was: hematitecalcium ferritemagnetiteglass phase. So the hematite and calcium ferrite should be development, and the glass phase should be inhabited in sinter on production. Minerals microhardness was connected with component elements and crystalline structure of the minerals besides ferrous content of sinter.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

725-729

Citation:

Online since:

February 2014

Keywords:

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Ruying Wang. Mei Shan Science and Technology, 1993(4): 12-13.

Google Scholar

[2] Tengjun Zuo. Foreign Sintering and Pelletizing, 1988(2): 27-28.

Google Scholar