Sealability Analysis of Aged Elastomer O-Rings for Usage in Solar Thermochemical Water-Splitting Reactors

Article Preview

Abstract:

Fluoroelastomer (FKM) and perfluoroelastomer (FFKM) O-rings are to be employed for the construction of a gate valve in a solar thermochemical water-splitting reactor for hydrogen production. To assess the O-rings’ sealing performance during the first stage of the gate valve’s closing process, the compressive response of the materials under the applied gate forces is determined. An accelerated ageing program at 200, 225 and 250 °C for FKM and 250, 275 and 300 °C for FFKM is performed on compressed O-rings and non-compressed O-ring segments for up to 14 days. The aged O-rings’ sealing performance at low forces, and hence at low compressive strain, is evaluated by conducting leakage rate tests in vacuum using a newly developed test stand. Experimental results provide for the tested O-rings data of a minimum compression necessary to guarantee efficient sealing at different thermo-oxidative ageing levels. To investigate the materials’ degradation extent, weight loss measurements are performed on the exposed O-ring segments. In all cases, cumulative weight loss increases with longer exposure times and higher temperatures, while the weight loss rate decreases with exposure time.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

37-48

Citation:

Online since:

March 2025

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2025 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] Zoller, S., Koepf, E., Nizamian, D., Stephan, M., Patané, A., Haueter, P., Romero, M.l, González-Aguilar, J., Lieftink, D., Wit, E., Brendelberger, S., Sizmann, A., and Steinfeld, A., "A solar tower fuel plant for the thermochemical production of kerosene from H2O and CO2." Joule Vol. 6 No. 7 (2022): p.1606–1616.

DOI: 10.1016/j.joule.2022.06.012

Google Scholar

[2] Brendelberger, S., Holzemer-Zerhusen, P., Vega Puga, E., Roeb, M., and Sattler, C., "Study of a new receiver-reactor cavity system with multiple mobile redox units for solar thermochemical water splitting." Solar Energy Vol. 235 (2022): p.118–128.

DOI: 10.1016/j.solener.2022.02.013

Google Scholar

[3] Battini, D., Donzella, G., Avanzini, A., Zenoni, A., Ferrari, M., Donzella, A., Pandini, S., Bignotti, F., Andrighetto, A., and Monetti, A., "Experimental testing and numerical simulations for life prediction of gate valve O-rings exposed to mixed neutron and gamma fields." Materials & Design Vol. 156 (2018): p.514–527.

DOI: 10.1016/j.matdes.2018.07.020

Google Scholar

[4] Kömmling, A., Jaunich, M., Goral, M., and Wolff, D., "Insights for lifetime predictions of O-ring seals from five-year long-term aging tests." Polymer Degradation and Stability Vol. 179 (2020): p.109278.

DOI: 10.1016/j.polymdegradstab.2020.109278

Google Scholar

[5] Kömmling, A., Jaunich, M., Pourmand, P., Wolff, D., and Hedenqvist, M., "Analysis of O-Ring Seal Failure under Static Conditions and Determination of End-of-Lifetime Criterion." Polymers Vol. 11 No. 8 (2019).

DOI: 10.3390/polym11081251

Google Scholar

[6] Kömmling, A., Jaunich, M., Pourmand, P., Wolff, D., and Gedde, U. W., "Influence of Ageing on Sealability of Elastomeric O‐Rings." Macromolecular Symposia Vol. 373 No. 1 (2017).

DOI: 10.1002/masy.201600157

Google Scholar

[7] Kader, M. A. and Bhowmick, A. K., "Thermal ageing, degradation and swelling of acrylate rubber, fluororubber and their blends containing polyfunctional acrylates." Polymer Degradation and Stability Vol. 79 No. 2 (2003): p.283–295.

DOI: 10.1016/S0141-3910(02)00292-6

Google Scholar

[8] Simon, A., Pepin, J., Berthier, D., and Méo, S., "Degradation mechanism of FKM during thermo-oxidative aging from mechanical and network structure correlations." Polymer Degradation and Stability Vol. 208 (2023): p.110271.

DOI: 10.1016/j.polymdegradstab.2023.110271

Google Scholar

[9] Sugama, T., Pyatina, T., Redline, E., McElhanon, J., and Blankenship, D., "Degradation of different elastomeric polymers in simulated geothermal environments at 300 °C." Polymer Degradation and Stability Vol. 120 (2015): p.328–339.

DOI: 10.1016/j.polymdegradstab.2015.07.010

Google Scholar

[10] Zhuo, W. Y., Wang, Q. L., Li, G., Yang, G., Zhang, H., Xu, W., Niu, Y. H., and Li, G. X., "Detection of the Destruction Mechanism of Perfluorinated Elastomer (FFKM) Network under Thermo-oxidative Aging Conditions." Chinese Journal of Polymer Science Vol. 40 No. 5 (2022): p.504–514.

DOI: 10.1007/s10118-022-2692-6

Google Scholar

[11] C. Otto Gehrckens GmbH & Co. KG, "Technisches Datenblatt Vi 665.". COG, Pinnenberg, Germany (2024). https://www.cog.de/uploads/tx_datenblattgenerator/pdf/de/vi-665.pdf.

Google Scholar

[12] C. Otto Gehrckens GmbH & Co. KG, "Technisches Datenblatt Perlast G75B.". COG, Pinnenberg, Germany (2021). https://www.cog.de/uploads/tx_datenblattgenerator/pdf/de/ perlast-g75b.pdf.

Google Scholar

[13] ISO 7743:2017, "Rubber, vulcanized or thermoplastic — Determination of compression stress-strain properties." International Organization for Standarization, Geneva, Switzerland. https://www.iso.org/standard/72784.html#lifecycle.

Google Scholar

[14] ISO 188:2023, "Rubber, vulcanized or thermoplastic — Accelerated ageing and heat resistance tests." International Organization for Standarization, Geneva, Switzerland. https://www.iso.org/standard/80468.html.

DOI: 10.3403/01316115u

Google Scholar

[15] Kömmling, A., "Alterung und Lebensdauervorhersage von O-Ring-Dichtungen." Dissertation. TU Berlin, Berlin, Germany.

Google Scholar

[16] Moore, D. F. and Geyer, W., "A review of hysteresis theories for elastomers." Wear Vol. 30 No. 1 (1974): p.1–34.

DOI: 10.1016/0043-1648(74)90055-6

Google Scholar

[17] C. Otto Gehrckens GmbH & Co. KG, "O-ring Basics: Everything about O-rings.". COG, Pinnenberg, Germany (2022). https://www.cog.de/fileadmin/dokumente/Broschueren/COG_ Broschuere_O-Ring_1x1_EN.pdf.

Google Scholar

[18] Eriks, "Technical Handbook of O-rings." (2024). https://o-ring.info/en/technical-info/technical-o-ring-handbook/.

Google Scholar

[19] ISO 48-4:2018, "Rubber, vulcanized or thermoplastic — Determination of hardness: Part 4: Indentation hardness by durometer method (Shore hardness)." International Organization for Standarization, Geneva, Switzerland. https://www.iso.org/standard/74969.html.

DOI: 10.3403/30373384u

Google Scholar

[20] Huang, X., Gu, J., Li, M., Yu, X., Liu, Y., and Xu, G., "A Leakage Prediction Model for Sealing Performance Assessment of EPDM O-Rings under Irradiation Conditions." Polymers Vol. 15 No. 14 (2023).

DOI: 10.3390/polym15143073

Google Scholar

[21] Yamada, Y. and Sogo, S., "Evaluation of Temperature Dependency of Gas Permeability on Various Kinds of Elastomers." Journal of the Vacuum Society of Japan Vol. 60 No. 12 (2017): p.502–506.

DOI: 10.3131/jvsj2.60.502

Google Scholar

[22] Hertz, D. L., "Evaluating thermal stability of fluoroelastomers via strain energy density." Sealing Technology Vol. 2005 No. 9 (2005): p.5–9.

DOI: 10.1016/S1350-4789(05)70895-3

Google Scholar