Fabrication of Zirconia Coating on the Surface of Al2O3-SiC-C Castable
Abstract:
Using zirconia Sol as zirconia source, zirconia coating has been fabricated on the surface of Al2O3-SiC-C castable by spraying technology after pretreated at 110oC, 300oC, 500oC, 700oC and 900oC. The oxidation resistance of Al2O3-SiC-C castable with zirconia coating was compared with that without coating, at the same time using microanalysis technique, effects of pretreatment temperatures and spraying times on the fabricated zirconia coating were investigated. Results suggest that better zirconia coating might be achieved after pretreated at 300oC and spraying one time. At this condition, fabricated zirconia coating has good continuity, closely bonded with substrate castable and even has a little penetration into the castable, and thus improved the oxidation resistance of Al2O3-SiC-C castable.
Info:
Periodical:
Pages:
82-86
Citation:
Online since:
January 2013
Authors:
Keywords:
Price:
Сopyright:
© 2013 Trans Tech Publications Ltd. All Rights Reserved
Share:
Citation: