Low Temperature Sintering of (Ca0.9375Sr0.0625)0.25(Li0.5Sm0.5)0.75TiO3 Microwave Dielectric Ceramics

Abstract:

Article Preview

The sintering behavior and microwave dielectric properties of the (Ca0.9375Sr0.0625)0.25(Li0.5Sm0.5)0.75TiO3 (CSLST) ceramics doped with different amounts of Li2O-B2O3-SiO2-CaO-Al2O3 (LBSCA) glass were investigated. The sintering temperature of the CSLST ceramics can be effectively reduced over 200oC due to the addition of LBSCA glass. For the 5 wt% LBSCA-doped CSLST ceramics, which are sintered at only 1000 oC for 5 h, show optimum microwave dielectric properties as follows: εr=84.74, Qf=2446 GHz and τf=-12.48 ppm/oC.

Info:

Periodical:

Materials Science Forum (Volumes 663-665)

Edited by:

Yuan Ming Huang

Pages:

1028-1031

DOI:

10.4028/www.scientific.net/MSF.663-665.1028

Citation:

Y. M. Li et al., "Low Temperature Sintering of (Ca0.9375Sr0.0625)0.25(Li0.5Sm0.5)0.75TiO3 Microwave Dielectric Ceramics", Materials Science Forum, Vols. 663-665, pp. 1028-1031, 2011

Online since:

November 2010