Dielectric and Ferroelectric Properties of (Pb0.9Ba0.1) ZrO3 Ceramics

Article Preview

Abstract:

(Pb1-xBax)ZrO3 (PBZ) ceramics for x = 0.10 were synthesized by the mixed oxide solid state reaction method. Phase transition was investigated by dielectric measurements in the temperature range from 27 to 350 °C at various frequencies. The permittivity of the solids corresponding to (Pb1-xBax) ZrO3 showed the maximum value of 10220 at x = 0.10 at the phase transition temperature. The maximum permittivity gradually increasing concentration up to x = 0.10. The ferroelectric hysteresis loop of the PBZ ceramics for x = 0.10 is displayed at room temperature and 0.2 Hz.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

247-250

Citation:

Online since:

June 2011

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2011 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] Y.J. Yu, Raj.N. Singh: J. Appl. Phys Vol. 88 (2000), p.7249.

Google Scholar

[2] M. -S. Yoon and H.M. Jang: J. Appl. Phys Vol. 77 (1995), p.3991.

Google Scholar

[3] S.E. Park and T.R. Shrout: Transactions on Ultrasonics, Ferroelectrics and Frequency Control Vol. 44 (1997), p.1140.

Google Scholar

[4] W.Y. Pan, C.Q. Dam, Q.M. Zhang and L.E. Cross: J. Appl. Phys Vol. 66 (1989), p.6014.

Google Scholar

[5] K. Uchino: Jpn. J. Appl. Phys Vol. 24 (1985), p.460.

Google Scholar

[6] B.P. Pokharel, M.K. Datta and D. Pandey: J. Mater. Sci Vol. 34 (1999), p.691.

Google Scholar

[7] B.P. Pokharel and D. Pandey: J. Appl. Phys Vol. 90 (2001), p.2985.

Google Scholar

[8] G. Rujijanagul, A. Rittidech and T. Bongkarn: Mater. Sci. Eng. A Vol. 438-440 (2006), p.360.

Google Scholar

[9] N. Vittayakorn, T. Bongkarn and G. Rujijanagul: Physica. B Vol. 387 (2007), p.415.

Google Scholar

[10] T. Bongkarn, G. Rujijanagul and S.J. Milne: Appl. Phys. Lett Vol. 92 (2008), p.092905.

Google Scholar

[11] B.P. Pokharel and D. Pandey: J. Appl. Phys Vol. 88 (2000), p.5364.

Google Scholar

[12] X.H. Hao, J.W. Zhai and X. Yao: J. Appl. Phys Vol. 104 (2008), p.124101.

Google Scholar

[13] L.J. Wu and J. M. Wu: J. Cryst. Growth Vol. 308 (2007), p.424.

Google Scholar

[14] I. El-Harrad, P. Becker, C. Carabatos-Nedelec, J. Handerek, Z. Ujma and D. Dmytrow: Vib. Spectrosc Vol. 10 (1996), p.301.

DOI: 10.1016/0924-2031(95)00034-8

Google Scholar

[15] T. Bongkarn and G. Rujijanagul: Curr. Appl. Phys Vol. 6 (2006), p.319.

Google Scholar

[16] T. Bongkarn, G. Rujijanagul and S.J. Milne: Mater. Sci Vol. 59 (2005), p.1200.

Google Scholar

[17] W.J. Mertz: Phys. Rev Vol. 91 (1953), p.513.

Google Scholar