Abstract:

Surface blistering during T6 heat treating is an artifact that is essentially unique to high pressure casting processes such as semi-solid casting and die casting. It is believed that the blistering originates from subsurface defects present in the castings. When the castings are exposed to elevated temperatures during solution heat treatment, the strength of the aluminum is reduced, and the defects expand to deform the surfaces of the castings. There are three potential sources for the subsurface defects - entrapped air, die lubricant or shot sleeve lubricant.This paper will report on a study to determine the origin of the defects present in the castings that produce the blisters. Along with attempting to separate the influence of air and the two types of lubricants on blister formation, the study will also examine the impact of a number of process parameters on blistering.

You might also be interested in these eBooks

Info:

Periodical:

Solid State Phenomena (Volume 256)

Pages:

192-198

Citation:

Online since:

September 2016

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2016 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] R.N. Lumley, R.G. O'donnell, D.R. Gunasegaram, M. Givord, U.S. Patent 8, 409, 374 B2 (2013).

Google Scholar

[2] R.N. Lumley, D.R. Gunasegaram, M. Gershenzon, R.G. O'Donnell, The Effect of Alloy Composition on Heat Treatment of Aluminum High Pressure Die Casting, 111th Metalcasting Congress (2007).

Google Scholar

[3] W.J. Tong, L. Qi, P.X. Qi, Study on Heat Treatment Blister of Squeeze Casting Parts, China Foundry 4 (2007) 108.

Google Scholar

[4] A. Kopper, Die Casting Plunger Lubricant Success Story: T6 Heat Treatable Die Castings, 113th NADCA Metalcasting Congress (2009) T09-023.

Google Scholar

[5] S.P. Midson, Minimizing Blistering During T6 Heat Treating of Semi-Solid Castings, Die Casting Engineer 55 (2011) 40-43.

DOI: 10.4028/www.scientific.net/ssp.256.192

Google Scholar

[6] Y. He, S. Midson, Q. Zhu, Impact of Die and Plunger Lubricants on Blistering during T6 Heat Treatment of Semi-Solid Castings, 2013 NADCA Die Casting Congress (2013).

DOI: 10.1002/9781118888100.ch4

Google Scholar

[7] Y. He, X. Xu, F. Zhang, D. Li, S. Midson, Q. Zhu, Influence of Process Parameters on Blistering During T6 Heat Treatment of Semi-Solid Castings, Shape Casting: 5th International Symposium 2014 (2013) 27.

DOI: 10.1002/9781118888100.ch4

Google Scholar

[8] X.G. Hu, F. Zhang, Y.F. He, S.P. Midson, Q. Zhu, Experimental Study and Numerical Simulation on the Blistering Defect during Thixocasting, Solid State Phenomena 217 (2015) 144-150.

DOI: 10.4028/www.scientific.net/ssp.217-218.144

Google Scholar