The Study of Bleaching Silk Sanitary Materials

Article Preview

Abstract:

The silk Sanitary Materials in hydrogen peroxide bleaching process, various experimental factors affect on the raw materials’ whiteness and tension. And through the single factor experiments and orthogonal test research and analysis, the significant influencing order of the whiteness of silk fiber is: temperature, concentration of hydrogen peroxide, and bleaching time; the significant influencing order of breaking tension is: bleaching time, temperature, and concentration of hydrogen peroxide. The optimum experimental program is as follows: hydrogen peroxide concentration of 22.5g / L, bleaching temperature of 80 °C, bleaching time, 60min, PH value of 9, sodium silicate concentration of 11.25g / L.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 175-176)

Pages:

765-768

Citation:

Online since:

January 2011

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2011 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

[1] J. Wang: Master degree thesis, Donghua University(2007).

Google Scholar

[2] D. Yang and H. Wang: Dyeing and finishing, Vol. 2(2007) p.44.

Google Scholar

[3] M. Huang: Dyeing and finishing, Vol. 1(1999)p.45.

Google Scholar

[4] M. Chen: Shanghai Textile Technology, Vol. 2(2002) p.31.

Google Scholar

[5] C. Zhang and J. Zhang: Tianjin Textile. Vol. 9(2005)p.37.

Google Scholar

[6] J. Zhu: Master degree thesis, Donghua University(2005).

Google Scholar