By an oxidation-reduction reaction the polyester film would be coated with a layer of tin. The conductivity of polyester film was discussed under different plating time, temperature, and PH. The results showed that when the plating time was 60 minutes, the temperature was 90°C and the PH was 4, the polyester film attained the optimal conductivity. The polyester film could be protected and the combination of magnetic and electrical conduction would be achieved by coating with a layer of magnetic powder after plating.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

96-100

Citation:

Online since:

December 2013

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2014 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] S.S. Guo: Necessity for Constituting Radiation Protection Apparel Standard. China Fiber Inspection Vol. 14(2010), pp.42-43.

Google Scholar

[2] M. Jalali, S. Dauterstedt, A. Michaud, et al. Wuthrich, Electromagnetic Shielding of Polymer-matrix Composites with Metallic Nanoparticles. Composites: Part B: Engineering, Vol. 42(2011), pp.1420-1426.

DOI: 10.1016/j.compositesb.2011.05.018

Google Scholar

[3] F. Yong: Development of Electromagnetic Shielding Fibers and Fabrics. Shandong Textile Science & Technology, Vol. 6(2009), pp.54-56.

Google Scholar

[4] D. Cao, Z.H. Li: Preparation of Silver-coated Glass Fiber by Electroless Plating with Ultrasonic Treatment. Materials Science and Engineering of Powder Metallurgy, Vol. 14(2009), pp.422-426.

Google Scholar

[5] F.D. Zhong, F.X. Zhong, Q.Y. Li, et al. Electromagnetic Shielding Paint and Preparation Method of Non Metallic Silver Powder, China. Patent 00112793. 4. (2001).

Google Scholar

[6] F.B. Yu, Y. Cheng: Preparation of Antibacterial Silver-plated Fiber and its Performance. Electroplating & Finishing , Vol. 31(2012), pp.36-38.

Google Scholar

[7] D.G. Guan, C.M. Sun, S.H. Zhong, et al. The Formula and Technology of Surface Tin Nickel Chemical Plating Glass Fiber, China, Patent 201010103214. 3. (2010).

Google Scholar

[8] W.S. Han, Y.X. Gu: An Slkyl Sulfonic Acid ChemicalTinning Solution and Tin Plating Process Based on the Chemical Tinning Solution, China, Patent 200910193997. 6. (2010).

Google Scholar

[9] X.X. Wang, W.M. Long, Y.Y. Pei, et al. Research of Electroless Tin Plating on Bag45CuZn Brazing Filler. Surface Technology, Vol 42(2013), pp.56-58.

Google Scholar

[10] Z.M. Qu, Q.G. Wang. Development of Conductive and Magnetic Shielding Composites. Materials Review, Vol. 25(2011), pp.138-141.

Google Scholar