Effect of Measurement Temperature on Electroluminescence Properties of PET Films

Abstract:

Article Preview

The Electroluminescence (EL) intensity and the spectrum of the of the PET films under different temperatures (77K, 296K, 353K) is tested, it is found that the pre-breakdown field under the low normal and high temperature of PET films is about 3.0MV/cm, 3.2MV/cm, 3.4MV/cm, respectively, and the formation of hot electron is not the main reason that cause aging and breakdown of PET films.

Info:

Periodical:

Edited by:

Ran Chen

Pages:

657-661

DOI:

10.4028/www.scientific.net/MSF.694.657

Citation:

J. Q. Lin et al., "Effect of Measurement Temperature on Electroluminescence Properties of PET Films", Materials Science Forum, Vol. 694, pp. 657-661, 2011