The Use of Hard Alloy Waste in Composite Galvanic Coatings for the Restoration of Car Parts

Article Preview

Abstract:

The results of the research of the use of powders based on tungsten carbide with a particle size of 1 μm or less, obtained by the method of electro-erosion dispersion from the waste of sintered hard alloys, as a dispersed phase of composite galvanic coatings based on iron during the restoration and hardening of car parts are presented. It is shown that the introduction powders of hard alloys of grades VK8 and T15K6 in the chloride electrolyte of iron plating with a concentration of 100 g/l and more, practically does not affect the micro-hardness, but allows to increase the relative wear resistance of the obtained composite galvanic coatings, compared to simple iron galvanic coatings, and, at the same time, increase the life of parts and reduce repair costs.

You might also be interested in these eBooks

Info:

Periodical:

Solid State Phenomena (Volume 299)

Pages:

258-263

Citation:

Online since:

January 2020

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2020 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] I.N. Borodin, Powder electroplating, Mechanical engineering, Moscow, (1990).

Google Scholar

[2] B.A. Semenikhin, L.P. Kuznetsova, R.A. Latypov, Restoration and strengthening of automotive parts with composite galvanic coatings using powders of hard alloys obtained by electroerosion dispersion, Works of GOSNITI. 109. Part 2 (2012) 57-60.

Google Scholar

[3] B.A. Semenikhin, L.P. Kuznetsova, Composite electroplated coatings for iron-based powders obtained by electroerosion dispersion of waste of hard alloys, Hardening technology and coatings. 4 (2014) 34-37.

Google Scholar

[4] B.A. Semenikhin, L.P. Kuznetsova, The use of powders of hard alloys as a dispersed phase in the restoration of car parts by iron plating, News SWSU. Techniques and technologies. 2. Part 1 (2012) 120-122.

Google Scholar

[5] Reference book of the technologist of car repair production. Under the editorship of G. A. Malyshev, Transport, Moscow, (1977).

Google Scholar

[6] E.V. Ageev, B.A. Semenikhin, E.V. Ageeva, R.A. Latypov, A study of the performance of the process of obtaining powders by a method of electroerosive dispersion, News KSTU. 4 (2010) 76-82.

Google Scholar

[7] E.V. Ageev, B.A. Semenikhin, R.A. Latypov, and V.I. Anikanov, Patent of Russia 2,449,859. (2010).

Google Scholar

[8] E.V. Ageev, B.A. Semenikhin and R.A. Latypov, Patent of Russia 2,455,117. (2009).

Google Scholar

[9] E.V. Ageev, B.A. Semenikhin and R.A. Latypov, Patent of Russia 2,424,382. (2009).

Google Scholar

[10] E.V. Ageev, R.A. Latypov, B.A. Semenikhin, E.V. Ageeva. Composition and properties of powders produced by electroerosion dispersion of waste of hard alloys, SWSU, Kursk, (2011).

Google Scholar

[11] E.V. Ageev, V.I. Serebrovsky, B.A. Semenikhin, E.V. Ageeva, R.A. Latypov, Yu.P. Gnezdilova, Restoration and strengthening of automotive parts equipment by plasma-powder surfacing with the use of powders obtained by electroerosion dispersion of sintered hard alloy wastes, KSAA, Kursk, (2010).

Google Scholar

[12] E.V. Ageev, V.I. Serebrovsky, R.A. Latypov, V.V. Serebrovsky, B.A. Semenikhin, E.V. Ageeva, Y.P. Gnezdilov, Restoration and strengthening of machine parts with composite galvanic coatings, KSAA. Kursk, (2011).

Google Scholar

[13] E.V. Ageev, V.N. Gadalov, B.A. Semenikhin, E.V. Ageeva, R.A. Latypov, X-ray diffraction of powders obtained by electroerosion dispersing of tungsten carbide, Procurement production in mechanical engineering. 2 (2011) 42-44.

Google Scholar

[14] E.V. Ageev, V.N. Gadalov, B.A. Semenikhin, E.V. Ageeva, R.A. Latypov, X-ray spectral microanalysis of powder particles obtained by electroerosion dispersion of a hard alloy, Hardening technologies and coatings. 2 (2011) 13-16.

Google Scholar

[15] E.V. Ageev, B.A. Semenikhin, E.V. Ageeva, R.A. Latypov, Evaluation of the effectiveness of the use of carbide powders obtained by electroerosion dispersion of hard alloy waste, in the restoration and hardening of parts by composite galvanic coatings, Hardening technologies and coatings. 9 (2011) 14-16.

Google Scholar

[16] E.V. Ageev, V.I. Serebrovsky, B.A. Semenikhin, E.V. Ageeva, R.A. Latypov, Study of the shape and surface morphology of powder particles used in the restoration and hardening of machine parts, Bulletin of Kursk State Agricultural Academy. 1 (2011) 72-75.

Google Scholar

[17] E.V. Ageev, B.A. Semenikhin, E.V. Ageeva, R.A. Latypov, Study of the chemical composition of powders obtained by electroerosion dispersion of a hard alloy, News of Southwest State University. 5-1 (2011) 138-144.

Google Scholar

[18] E.V. Ageev, B.A. Semenikhin, R.A. Latypov, Preparation of nanopowder based on tungsten carbide and application for recovery and hardening of machine parts, News of Samara scientific center of Russian Academy of Sciences. 12. Ch.1-2 (2010) 273-275.

Google Scholar

[19] E.V. Ageev, V.N. Gadalov, B.A. Semenikhin, E.V. Ageeva, R.A. Latypov, Obtaining wear-resistant powders from hard alloy waste, Procurement production in mechanical engineering. 12 (2010) 39-44.

Google Scholar

[20] E.V. Ageev, B.A. Semenikhin, E.V. Ageeva, R.A. Latypov, N.A. Pivovar, Study of the performance of the process of obtaining powders by a method of electroerosive dispersion, News of Kursk State Technical University. 4 (2010). 76-82.

Google Scholar

[21] R.A. Latypov, A.B. Korostelev, E.V. Ageev, B.A. Semenikhin, The properties of powders from waste hard alloys VK8 and T15K6 obtained by electroerosive dispersion, All materials. Encyclopedic reference book. 7 (2010) 2-6.

Google Scholar

[22] E.V. Ageev, B.A. Semenikhin, R.A. Latypov, Method for producing nanostructured powders based on the WC-CO system and a device for its implementation, Fundamental and applied problems of engineering and technology. 5 (2010) 39-42.

Google Scholar

[23] E.F. Nemilov, Electroerosive treatment of materials, Mechanical Engineering, Leningrad, (1983).

Google Scholar