Effect of Pre-Calcined Method on Dielectric, Ferroelectric, and Piezoelectric Properties of Lead-Free Piezoelectric Lix(K0.5Na0.5)1-x(Nb0.8Ta0.2)O3 Ceramics
Abstract:
The structure and electrical characteristics of the lead-free Lix(K0.5Na0.5)1-x(Nb0.8Ta0.2)O3 (x=0~0.05) piezoelectric ceramics for the conventional solid-state reaction method and the B-side pre-calcined method were achieved and compared. For the B-side pre-calcined method, the lead-free ceramic material exhibited the excellent electrical and piezoelectric properties. The relative dielectric constant (εr) and loss (tan δ) of the Lix(K0.5Na0.5)1-x(Nb0.8Ta0.2)O3 for x=0.03 using the B-side pre-calcined method were 1223 and 0.021, respectively. In addition, the electromechanical coupling factors (kp) and Curie temperature (Tc) was 48.5 % and 315°C. Finally, the electrical properties of the lead-free Lix(K0.5Na0.5)1-x(Nb0.8Ta0.2)O3(x=0~0.05) homogeneity ceramics improved by the B-side pre-calcined method were also investigated and discussed.
Info:
Periodical:
Pages:
1218-1221
Citation:
Online since:
June 2012
Price:
Сopyright:
© 2012 Trans Tech Publications Ltd. All Rights Reserved
Share:
Citation: