New Crystallographic Textures of Nd2Fe14B/α-Fe Nanocomposite Materials Prepared by Controlled Melt Spinning

Abstract:

Article Preview

In Nd9.5Fe84B6.5 melt-spun ribbon, the quenching temperature is found to be effective for the texture development of Nd2Fe14B nanocrystals. For a relatively low quenching temperature of 1250°C a (00l) texture of Nd2Fe14B crystals was found on the free-side surface of the ribbons. At a higher quenching temperature of 1350°C, the microstructure of the free-side surface of the ribbons switches into (320) and (517) texture. It is believed that the transformation of the melt at higher temperature triggers the switch of the texture.

Info:

Periodical:

Materials Science Forum (Volumes 654-656)

Main Theme:

Edited by:

Jian-Feng Nie and Allan Morton

Pages:

1170-1173

DOI:

10.4028/www.scientific.net/MSF.654-656.1170

Citation:

X. R. Zeng et al., "New Crystallographic Textures of Nd2Fe14B/α-Fe Nanocomposite Materials Prepared by Controlled Melt Spinning", Materials Science Forum, Vols. 654-656, pp. 1170-1173, 2010

Online since:

June 2010

Export:

Price:

$35.00

In order to see related information, you need to Login.

In order to see related information, you need to Login.