Abstract:

The paper presents the data obtained in the course of experimental studies on the production of rods from the Al-0.5% REM alloy using combined processing methods, such as combined rolling-extruding (CRE) and combined casting and rolling-extruding (CCRE). The variable parameters were the temperature of the ingot or melt, the degree of deformation and the strain rate. With the help of strain gauge equipment, experimental data were obtained on the forces acting on the rolls and the die of the CCRE-200 combined processing unit in the process of obtaining rods with a diameter of 5 and 9 mm. The estimation of the dependence of the mechanical properties of the rods on the variable factors has been carried out. The highest strength properties are possessed by a bar obtained by the CRE mode at a temperature T = 550 oC and a strain rate ξ = 0.74 s-1. When comparing the temperature of pouring the metal, the highest strength properties are possessed by a rod with a diameter of 9 mm and 5 mm and a strain rate ξ = 0.74 s-1. If compare in terms of the deformation rate, then the highest strength properties are possessed by a rod with a diameter of 5 mm and a deformation rate ξ = 1.49 s-1. The plasticity of deformed semi-finished products in all modes is at a high level, which allows further processing.

You might also be interested in these eBooks

Info:

Periodical:

Pages:

262-268

Citation:

Online since:

May 2021

Export:

Price:

Permissions CCC:

Permissions PLS:

Сopyright:

© 2021 Trans Tech Publications Ltd. All Rights Reserved

Share:

Citation:

* - Corresponding Author

[1] D.I. Belyy, Aluminium alloys for leads of cable products, Kabeli i Provoda. 1 (2012) 8-15.

Google Scholar

[2] Yu.A. Gorbunov, The Role and Prospects of Rare Earth Metals in the Development of Physical-Mechanical Characteristics and Applications of Deformable Aluminum Alloys, Journal of Siberian Federal University. Engineering & Technologies. 8(5) (2015) 636-645.

DOI: 10.17516/1999-494x-2015-8-5-636-645

Google Scholar

[3] D.A. Chernavina, E.A. Chernavin, A.V. Faller, M.Yu. Zdanovich, Global aluminum market: development trends, prospects and key problems, Molodoy uchenyy. 17 (2018) 206-210.

Google Scholar

[4] A. Tukker, Rare earth elements supply restrictions: Market failures, not scarcity, hamper their current use in high-tech applications, Environ. Sci. Technol. 48 (2014) 9973-9974.

DOI: 10.1021/es503548f

Google Scholar

[5] V.G. Shmorgun, L.M. Gurevich, A.F. Trudov, S.P. Pisarev et al., Mechanical properties of wire with a carrier layer of aluminum alloy 01417, Izvestiya VolGTU. 136(9) (2014) 109-113.

Google Scholar

[6] V.S. Sudavtsova, M.A. Shevchenko, V.V. Berezutskiy, M.I. Ivanov, I.V. Mateyko, V.G. Kudin, Thermodynamic properties and phase equilibria in alloys of Al (Si)–Ce binary systems, Journal of Physical Chemistry. 88(5) (2014) 736-746.

Google Scholar

[7] A. Mogucheva, D. Zyabkin, R. Kaibyshev, Effect of the thermomechanical processing on microstructure and properties of an Al-Ce alloy, Materials Science Forum. 706-709 (2012) 361-366.

DOI: 10.4028/www.scientific.net/msf.706-709.361

Google Scholar

[8] S.B. Sidelnikikov, N.N. Dovzhenko, N.N. Zagirov. Combined and complex methods of machining non-ferrous metals and alloys, M.: MAKS PRESS, (2005).

Google Scholar

[9] S.B. Sidelnikikov, N.N. Dovzhenko, V.N. Timofeev et al., RF Patent 67492. (2007).

Google Scholar

[10] S.B. Sidelnikov, D.S. Voroshilov, M.V. Pervukhin, M.M. Motkov, Development and research of technology for producing electrotechnical wire from alloys of the Al – REM system, obtained with the application of combined machining methods, Tsvetnye metally. 9 (2019) 63-68.

DOI: 10.17580/tsm.2019.09.10

Google Scholar

[11] S. Sidelnikov, D. Voroshilov, M. Motkov, M. Voroshilova, V. Bespalov, Development of Combined Machining Modes, Investigation of Mechanical Properties and Structure of Deformed Semi-Finished Products from Alloy 01417, Materials Science Forum. 992 (2020) 498-503.

DOI: 10.4028/www.scientific.net/msf.992.498

Google Scholar

[12] N.A. Belov, A.N. Alabin, A.R. Teleuova, Comparative analysis of alloying additives as applied to the production of heat-resistant aluminum-base wires, Metal Science and Heat Treatment. 53(9-10) (2012) 455-459.

DOI: 10.1007/s11041-012-9415-5

Google Scholar

[13] H. Liao, Y. Wu, Y. Wang, Microstructure Evolution of Al-0.35%Si-0.2%Mg-0.3%Ce Alloy During Hot Extrusion and Its Contributions to Performances, Journal of Materials Engineering and Performance. 24(6) (2015) 2503-2510.

DOI: 10.1007/s11665-015-1485-2

Google Scholar

[14] H. Liao, Y. Liu, C. Lü, Q. Wang, Mechanisms for Ce-induced remarkable improvement of conductivity in Al alloys, Journal of Materials Research. 32(3) (2017) 566-574.

DOI: 10.1557/jmr.2016.477

Google Scholar

[15] M. Zhang, H. Wang, W. Han, M. Zhang, Yu. Li, Ya. Wang, Yu. Xue, F. Ma, X. Zhang. Electrochemical extraction of cerium and formation of Al–Ce alloy from CeO2 assisted by AlCl3 in LiCl–KCl melts, Sci China Chem. 57(11) (2014) 1477-1482.

DOI: 10.1007/s11426-014-5214-8

Google Scholar

[16] Z.M. Shi, K. Gao, Y.T. Shi, Y. Wang, Microstructure and mechanical properties of rare-earth-modified Al−1Fe binary alloys, Materials Science and Engineering: A. 632 (2017) 62-71.

DOI: 10.1016/j.msea.2015.02.068

Google Scholar

[17] S.B. Sidelnikov, N.N. Dovzhenko, T.N. Drozdova et al., Investigation of the structure and assessment of properties of cast and deformed semifinished products from alloys of the Al-REM system with different nickel content, Vestnik of Nosov Magnitogorsk State Technical University. 1 (2013) 45-48.

Google Scholar

[18] X. Huang, H. Yan, Effect of trace La addition on the microstructure and mechanical property of as-cast ADC12 Al-Alloy, J. Wuhan Univ. Technol.-Materials Sci. Ed. 28 (2013) 202-205.

DOI: 10.1007/s11595-013-0665-x

Google Scholar

[19] P. Li, Z. Wu, Y. Wang, X. Gao, Z. Wang, Zh. Li, Effect of cerium on mechanical performance and electrical conductivity of aluminum rod for electrical purpose, J. Rare Earths. 24 (2006) 355–-357.

DOI: 10.1016/s1002-0721(07)60400-1

Google Scholar

[20] Ch.-L. Lv, H. Liao, Ye Liu, Q. Wang, Effect of Ce on castability, mechanical properties and electric conductivity of commercial purity aluminum, China Foundry. 12 (2015) 277-284.

Google Scholar

[21] X. Cao, Sh. Wang, Yi Wang, The effect of annealing and aging on the high temperature internal friction spectra of Al-Ce alloy, Mater. Sci. Eng. B. 163 (2009) 174-178.

DOI: 10.1016/j.mseb.2009.05.030

Google Scholar

[22] A.E. Medvedev, M.Y. Murashkin, N.A. Enikeev, I. Bikmukhametov, R.Z. Valiev, P.D. Hodgson, R. Lapovok, Effect of the eutectic Al-(Ce,La) phase morphology on microstructure, mechanical properties, electrical conductivity and heat resistance of Al-4.5(Ce,La) alloy after SPD and subsequent annealing, Journal of Alloys and Compounds. 796 (2019) 321-330.

DOI: 10.1016/j.jallcom.2019.05.006

Google Scholar